Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 51.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
CTE, linear, Parallel to Flow | 51.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
CTE, linear, Parallel to Flow | 51.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
CTE, linear, Parallel to Flow | 51.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
CTE, linear, Parallel to Flow | 51.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
CTE, linear, Parallel to Flow | 51.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |