Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature <=143 °C |
2.78 µin/in-°F @Temperature <=289 °F |
Below Tg; ISO 11359 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature <=143 °C |
2.78 µin/in-°F @Temperature <=289 °F |
Below Tg; ISO 11359 |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature <=143 °C |
2.78 µin/in-°F @Temperature <=289 °F |
Below Tg; ISO 11359 |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature >=143 °C |
2.78 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature <=152 °C |
2.78 µin/in-°F @Temperature <=306 °F |
Below Tg; ISO 11359 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
CTE, linear, Parallel to Flow | 5.00 µm/m-°C @Temperature >=152 °C |
2.78 µin/in-°F @Temperature >=306 °F |
Above Tg; ISO 11359 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |