Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS Noryl* NH7010 resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight parts.. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS Noryl* NH7010 resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight parts.. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS (Asia Pacific) High heat, Non halogenated flame retardant Noryl product |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS (Asia Pacific) High heat, Non halogenated flame retardant Noryl product |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
CTE, linear, Parallel to Flow | 81.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |