Polymer Property : CTE, linear, Parallel to Flow = 45.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Below Tg; ISO 11359
Victrex® PEEK 450G General Purpose
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac..
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature <=152 °C
25.0 µin/in-°F

@Temperature <=306 °F
Below Tg; ISO 11359
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature <=162 °C
25.0 µin/in-°F

@Temperature <=324 °F
Below Tg; ISO 11359
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, ..
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL V02570 PPE+HIPS
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DE0039 PC
LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DE0039 PC
LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 815 PBT
15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 815F PBT+PET
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 855 PBT
15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 855 PBT (Asia Pacific)
15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 95.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® 1760 PBT+PC
11% Glass Reinforced PBT+PC alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp EB004 PEI
LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp EB004 PEI (Asia Pacific)
LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific)
LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific)
LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp YF006 TPEE
LNP THERMOCOMP* YF006 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific)
LNP* Stat-kon* DE0039 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific)
LNP* Stat-kon* DE0039 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific)
15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 815F PBT+PET (Asia Pacific)
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT (Asia Pacific)
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT (Asia Pacific)
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Asia Pacific)
PPE+PS blend. 10% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including wate..
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Below Tg; ISO 11359
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..
CTE, linear, Parallel to Flow 45.0 µm/m-°C

@Temperature <=143 °C
25.0 µin/in-°F

@Temperature <=289 °F
Below Tg; ISO 11359
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac..