Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC LNP* LUBRICOMP* DL001 is a compound based on Polycarbonate resin containing 5% PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Asia Pacific) LNP* Lubricomp* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America.. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC (Asia Pacific) LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DL003EU PC LNP LUBRICOMP* DL003EU is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, UV Stabilized, Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 LNP* LUBRICOMP* RAL22S is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 (Asia Pacific) LNP* Lubricomp* RAL22S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 LNP* LUBRICOMP* RFL36L is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 (Asia Pacific) LNP* Lubricomp* RFL36L is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer (Asia Pacific) LNP* THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific) LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
CTE, linear, Parallel to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, Internally Lubricated |