Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI
LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated.
CTE, linear, Parallel to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI
LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated.
CTE, linear, Parallel to Flow 39.0 µm/m-°C

@Temperature -40.0 - 150 °C
21.7 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 4002 PEI
PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL 94 V0 and 5VA listing in recognized colors.
CTE, linear, Parallel to Flow 39.0 µm/m-°C

@Temperature 23.0 - 150 °C
21.7 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 4002 PEI
PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL 94 V0 and 5VA listing in recognized colors.
CTE, linear, Parallel to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® 1760E PBT+PC
11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin.
CTE, linear, Parallel to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® 1760E PBT+PC
11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin.
CTE, linear, Parallel to Flow 39.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced
CTE, linear, Parallel to Flow 39.0 µm/m-°C

@Temperature 150 - 200 °C
21.7 µin/in-°F

@Temperature 302 - 392 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)  (discontinued **)
Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, ..