Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 69.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
CTE, linear, Parallel to Flow | 69.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Asia Pacific) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
CTE, linear, Parallel to Flow | 69.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Asia Pacific) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD103R PC FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD103R PC (Asia Pacific) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD103R PC (Europe-Africa-Middle East) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD104R PC FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD104R PC (Europe-Africa-Middle East) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
CTE, linear, Parallel to Flow | 69.6 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXM141R PC FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
CTE, linear, Parallel to Flow | 69.6 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
CTE, linear, Parallel to Flow | 69.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD104R PC (Asia Pacific) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
CTE, linear, Parallel to Flow | 69.6 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXM141R PC (Asia Pacific) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |