Polymer Property : CTE, linear, Parallel to Flow = 3.00 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 5.40 µm/m-°C

@Temperature -40.0 - 40.0 °C
3.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES
LNP* THERMOCOMP* JF003XXZ is a compound based on Polyethersulfone resin containing 15% Glass Fiber.
CTE, linear, Parallel to Flow 5.40 µm/m-°C

@Temperature -40.0 - 40.0 °C
3.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES (Asia Pacific)
LNP* Thermocomp* JF003XXZ is a compound based on Polyethersulfone resin containing Glass Fiber.
CTE, linear, Parallel to Flow 5.40 µm/m-°C

@Temperature -40.0 - 40.0 °C
3.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK
LNP* THERMOCOMP* LF005 is a compound based on Polyetheretherketone resin containing 25% Glass Fiber.
CTE, linear, Parallel to Flow 5.40 µm/m-°C

@Temperature -40.0 - 40.0 °C
3.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK (Asia Pacific)
LNP* Thermocomp* LF005 is a compound based on Polyetheretherketone resin containing Glass Fiber.