Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific)
LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.This data was suppli..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature 50.0 - 100 °C
14.4 µin/in-°F

@Temperature 122 - 212 °F
4
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral
Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
14.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS
LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability.
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature 23.0 - 150 °C
14.4 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2100 PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature 23.0 - 150 °C
14.4 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature 23.0 - 150 °C
14.4 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU2100 PEI (Europe-Africa-Middle East)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature 100 - 150 °C
14.4 µin/in-°F

@Temperature 212 - 302 °F
4
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
14.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultrason S 2010 G4 20% Glass Filled PSU
Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Thickness 4.00 mm,
Temperature 25.0 °C
14.4 µin/in-°F

@Thickness 0.157 in,
Temperature 77.0 °F
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Thickness 4.00 mm,
Temperature 75.0 °C
14.4 µin/in-°F

@Thickness 0.157 in,
Temperature 167 °F
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
Copyright © lookpolymers.com All Rights Reserved