Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36 PA6.12 LNP LUBRICOMP* IFL36 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 420 PBT (Asia Pacific) 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature 60.0 - 138 °C |
14.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 420 PBT (Asia Pacific) 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 420HP PBT 30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 420M PBT (Asia Pacific) 30% GR PBTP. Easy flow/release. High stiffness and load bearing properties.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 420R PBT (Asia Pacific) 30% GR, ex strength/stiffness/dimensional stability; heat resistance. Appliance handles, spotlights, electric motors, etc. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 732E PBT + PC + PET 30% glass/mineral reinforced, excellent thermal performance, low shrinkage and warp. Easy flow. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature 60.0 - 138 °C |
14.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 732E PBT + PC + PET 30% glass/mineral reinforced, excellent thermal performance, low shrinkage and warp. Easy flow. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 735 PBT 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific) 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature 60.0 - 138 °C |
14.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 735 PBT+PET 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 780 PBT 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 830 PBT 30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature 60.0 - 138 °C |
14.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 830 PBT 30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature 60.0 - 138 °C |
14.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 830 PBT (Asia Pacific) 30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RF008H PA 66 LNP* THERMOCOMP* RF008H is a compound based on Nylon 66 containing 40% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RX10405H PA 66 LNP* Thermocomp* RX10405H is a compound based on Nylon 6/6 containing Carbon Fiber. Characteristics of this grade are: Healthcare. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp WC003P Polyester Elastomer LNP* Thermocomp* WC003P is a compound based on Polyester resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature 60.0 - 138 °C |
14.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 420SE0U PBT (Asia Pacific) UV-Stabilized version of 420SE0. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 732E PBT 30% glass/mineral reinforced, excellent thermal performance, low shrinkage and warp. Easy flow.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® HX420HP PBT Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature 60.0 - 138 °C |
14.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® HX420HP PBT Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature 60.0 - 138 °C |
14.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East) Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp 2C004 LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC (Asia Pacific) LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF PX06417 PA 6 LNP THERMOTUF* PX06417 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF PX06417 PA 6 LNP THERMOTUF* PX06417 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications. |