Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific)
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific)
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East)
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East)
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS
Reinforced PC/ABS with high stiffness and low CTE.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS
Reinforced PC/ABS with high stiffness and low CTE.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific)
Reinforced PC/ABS with high stiffness and low CTE.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific)
Reinforced PC/ABS with high stiffness and low CTE.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Europe-Africa-Middle East)
Reinforced PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Europe-Africa-Middle East)
Reinforced PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
23.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics REMEX VR4831 PBT
15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics REMEX VR4831 PBT
15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4870HH PC+PET
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
23.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS
LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
23.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly
LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X5630 PC+PET
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature 200 - 250 °C
23.9 µin/in-°F

@Temperature 392 - 482 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)  (discontinued **)
Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, ..
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications