Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12
LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber.
CTE, linear, Parallel to Flow 40.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.5 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12
LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber.
CTE, linear, Parallel to Flow 40.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.5 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific)
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci..
CTE, linear, Parallel to Flow 40.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.5 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12