Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 2.78 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 5.00 µm/m-°C

@Temperature <=143 °C
2.78 µin/in-°F

@Temperature <=289 °F
Below Tg; ISO 11359
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
CTE, linear, Parallel to Flow 5.00 µm/m-°C

@Temperature <=143 °C
2.78 µin/in-°F

@Temperature <=289 °F
Below Tg; ISO 11359
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
CTE, linear, Parallel to Flow 5.00 µm/m-°C

@Temperature <=143 °C
2.78 µin/in-°F

@Temperature <=289 °F
Below Tg; ISO 11359
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont..
CTE, linear, Parallel to Flow 5.00 µm/m-°C

@Temperature >=143 °C
2.78 µin/in-°F

@Temperature >=289 °F
Above Tg; ISO 11359
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont..
CTE, linear, Parallel to Flow 5.00 µm/m-°C

@Temperature <=152 °C
2.78 µin/in-°F

@Temperature <=306 °F
Below Tg; ISO 11359
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
CTE, linear, Parallel to Flow 5.00 µm/m-°C

@Temperature >=152 °C
2.78 µin/in-°F

@Temperature >=306 °F
Above Tg; ISO 11359
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
Copyright © lookpolymers.com All Rights Reserved