Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature >=143 °C |
13.9 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
13.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 150 °C |
13.9 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem 2200N PEI 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 150 °C |
13.9 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 150 °C |
13.9 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2210K PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 150 °C |
13.9 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 150 °C |
13.9 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 150 °C |
13.9 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 0.000 - 100 °C |
13.9 µin/in-°F @Temperature 32.0 - 212 °F |
2 |
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in wat.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -20.0 - 150 °C |
13.9 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM HU2200 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 420SE0U PBT PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX01303C PC LNP STAT-KON* DX01303C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East) VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 830F PBT+PET (Europe-Africa-Middle East) PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East) Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ420HP PBT Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Asia Pacific) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
13.9 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
13.9 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
13.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FE1630PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1630PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |