Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature <=143 °C
7.22 µin/in-°F

@Temperature <=289 °F
Below Tg; ISO 11359
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac..
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature >=162 °C
7.22 µin/in-°F

@Temperature >=324 °F
Above Tg; ISO 11359
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, ..
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature -40.0 - 150 °C
7.22 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 150 °C
7.22 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature -40.0 - 150 °C
7.22 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 150 °C
7.22 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 150 - 250 °C
7.22 µin/in-°F

@Temperature 302 - 482 °F
2
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 150 °C
7.22 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM SF2360 PEI Blend (Asia Pacific)
High flow Ultem for thin wall application
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 150 °C
7.22 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East)
DATA ON BK1005 ONLY.
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 150 °C
7.22 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+PS
DATA ON BK1005 ONLY.
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature -40.0 - 150 °C
7.22 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX152R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 23.0 - 150 °C
7.22 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX152R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 180 °C
7.22 µin/in-°F

@Temperature 356 °F
DIN 53752
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
CTE, linear, Parallel to Flow 13.0 µm/m-°C

@Temperature 149 - 249 °C
7.22 µin/in-°F

@Temperature 300 - 480 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature..
Copyright © lookpolymers.com All Rights Reserved