Polymer Property : CTE, linear, Parallel to Flow = 12.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature 100 - 200 °C
6.67 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th..
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
6.67 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK
LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
6.67 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT
LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
6.67 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT
LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
6.67 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON UX03320 PPA
LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural.
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
6.67 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON UX03320 PPA
LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural.
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
6.67 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
6.67 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
6.67 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
6.67 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.