Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX MS003 PP LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12 LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Asia Pacific) PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON MFD03 PP LNP* STAT-KON* MFD03 is a compound based on Polypropylene resin containing 15% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 104 µm/m-°C @Temperature -40.0 - 40.0 °C |
57.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON MFD03 PP (Asia Pacific) LNP* Stat-kon* MFD03 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |