Thermal Properties | Metric | English | Comments |
---|---|---|---|
Hot Ball Pressure Test | <= 150 °C | <= 302 °F | IEC 60695-10-2 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Hot Ball Pressure Test | <= 150 °C | <= 302 °F | IEC 60695-10-2 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Hot Ball Pressure Test | <= 150 °C | <= 302 °F | IEC 60695-10-2 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |