Thermal Properties | Metric | English | Comments |
---|---|---|---|
Hot Ball Pressure Test | <= 80.0 °C | <= 176 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East) CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Hot Ball Pressure Test | <= 80.0 °C | <= 176 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Hot Ball Pressure Test | 80.0 - 105 °C | 176 - 221 °F | Average value: 95.0 °C Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Hot Ball Pressure Test | 80.0 - 100 °C | 176 - 212 °F | Average value: 94.5 °C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Hot Ball Pressure Test | 80.0 °C @Thickness 2.00 mm |
176 °F @Thickness 0.0787 in |
IEC695-10-2 |
Kingfa FRHIPS-1162 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.6mm, V-2 @ 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingEl.. |
|||
Hot Ball Pressure Test | <= 80.0 °C | <= 176 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Noryl V190 PPE+HIPS (Europe-Africa-Middle East) NORYL V190 is an unfilled flame retardant material with a Vicat B/120 of 90°C according ISO 306. NORYL V190 is V1 at 2.0 mm according UL94 and halogen free according VDE/DIN 472 part 815.This dat.. |
|||
Hot Ball Pressure Test | 80.0 °C @Thickness 2.00 mm |
176 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXATEC 6120 AES SAXATEC 6120 is a easy lowing, weatherable AES injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym.. |
|||
Hot Ball Pressure Test | 80.0 °C @Thickness 2.00 mm |
176 °F @Thickness 0.0787 in |
IE/CEN 60335-1 |
Sax Polymers SAXLAC 420HI Acrylonitrile Butadiene Styrene Saxalac 420HI is a flame retardant, very high flow ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provided.. |
|||
Hot Ball Pressure Test | 80.0 °C | 176 °F | JET, 2.0 mm |
Total PSI 3341 High Impact Polystyrene Total Petrochemicals Polystyrene 3341 is a high impact polystyrene for the extrusion industry. Its good mechanical and thermal properties leads to the production of thermoformed articles of good ri.. |
|||
Hot Ball Pressure Test | >= 80.0 °C | >= 176 °F | BS 3456, IEC 335 |
EPICHEM Epilac ABS Acrylonitrile Butadiene Styrene |
|||
Hot Ball Pressure Test | >= 80.0 °C | >= 176 °F | BS 3456, IEC 335 |
EPICHEM Epilac R ABS 10% GF Acrylonitrile Butadiene Styrene, 10% Glass Fiber Characteristics: 10% glass fibre filled |
|||
Hot Ball Pressure Test | >= 80.0 °C | >= 176 °F | BS 3456, IEC 335 |
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber Characteristics: 17% glass fibre filled |