Thermal Properties Metric English Comments
Liquidus 1343 °C
2449 °F
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725) Age Hardened Strip
Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Strip samples. Other property values are typical of INCONEL® alloy 725.D..
Liquidus 1343 °C
2449 °F
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round
Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D..
Liquidus 1343 °C
2449 °F
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Tube
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Age Hardened Tube samples. Other property values are typical of INCONEL® alloy 725.Data provi..
Liquidus 1343 °C
2449 °F
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Round
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Round samples. Other property values are typical of INCONEL® alloy 725.Data provided..
Liquidus 1343 °C
2449 °F
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Tube
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Tube samples. Other property values are typical of INCONEL® alloy 725.Data provided ..
Liquidus 1343 °C
2449 °F
Special Metals INCONEL® G-3 Nickel Superalloy
Data provided by the manufacturer, Special Metals.
Liquidus 1343 °C
2449 °F
ATI Allvac® 718Plus™ Nickel Superalloy
Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the..