Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.960 - 1.06 W/m-K @Temperature 1400 °C |
6.66 - 7.36 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast CURAS 50 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre.. |
|||
Thermal Conductivity | 0.960 - 1.06 W/m-K @Temperature 1400 °C |
6.66 - 7.36 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast CURAS 40 D Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of special additions this type of moldable has already a reasonabl.. |
|||
Thermal Conductivity | 0.960 - 1.06 W/m-K @Temperature 1400 °C |
6.66 - 7.36 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast CURAS 40 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre.. |
|||
Thermal Conductivity | 0.960 - 1.06 W/m-K @Temperature 1400 °C |
6.66 - 7.36 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast CURAS 50 D Moldable Refractory Material Description: Because of special additions this moldable already has a reasonable strength at room temperature. This material is supplied as a dry powder, it has to be mixed with potable water to the.. |
|||
Thermal Conductivity | 0.960 - 1.06 W/m-K @Temperature 1000 °C |
6.66 - 7.36 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast CURON 13 S Dense Refractory Castable Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol.. |
|||
Thermal Conductivity | 0.960 - 1.06 W/m-K @Temperature 1000 °C |
6.66 - 7.36 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast CURON 13 SC Dense Refractory Castable Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/ho.. |