Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 2.57 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.370 W/m-K

@Temperature 100 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 212 °F
Pyrotek NAD-11 Structural Insulation Board
NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation ..
Thermal Conductivity 0.370 W/m-K

@Temperature 1095 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 2003 °F
Pyrotek SF-50 Foamed Fused Silica Insulation Board
SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o..
Thermal Conductivity 0.370 W/m-K

@Temperature 250 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company
Thermal Conductivity 0.370 - 0.470 W/m-K

@Temperature 100 °C
2.57 - 3.26 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Thermal Conductivity 0.370 - 0.470 W/m-K

@Temperature 200 °C
2.57 - 3.26 BTU-in/hr-ft²-°F

@Temperature 392 °F
Gouda Vuurvast FI 45-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.370 - 0.470 W/m-K

@Temperature 100 °C
2.57 - 3.26 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 125 GM Refractory Insulating Castable
Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast...
Thermal Conductivity 0.370 - 0.470 W/m-K

@Temperature 600 °C
2.57 - 3.26 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 135 Refractory Insulating Castable
Description: Golite 135 can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning vari..
Thermal Conductivity 0.370 W/m-K

@Temperature 1093 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 1999 °F
ASTM C182
BNZ Materials BNZ-26 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.370 W/m-K

@Temperature 816 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials BNZ-28 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.370 W/m-K

@Temperature 1000 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 1830 °F
ASTM C182
BNZ Materials Color A Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.370 W/m-K

@Temperature 1093 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 1999 °F
ASTM C182
BNZ Materials PA 23 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.370 - 0.470 W/m-K

@Temperature 100 °C
2.57 - 3.26 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 135 GM Refractory Insulating Castable
Description: This gunning material can be used in direct contact with open fire and has a high strength.Remarks: These values were obtained from cast samples. These values apply to cast products.Inf..