Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 17.5 W/m-K @Temperature 600 °C |
121 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 600 °C |
121 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 300 °C |
121 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Ultimet® alloy, 1.6 mm sheet Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 300 °C |
121 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 300 °C |
121 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 300 °C |
121 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 316°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 300 °C |
121 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 300 °C |
121 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Ultimet® alloy, all-weld metal, GTAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 300 °C |
121 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Ultimet® alloy, all-weld metal, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 300 °C |
121 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Ultimet® alloy, plate, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, 50% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 600 °C |
121 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 600 °C |
121 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Thermal Conductivity | 17.4 W/m-K @Temperature 300 °C |
121 BTU-in/hr-ft²-°F @Temperature 572 °F |
Annealed Condition |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 700 °C |
121 BTU-in/hr-ft²-°F @Temperature 1290 °F |
Hardened Condition |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, SMAW weldment, 19.1 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 600 °C |
121 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Thermal Conductivity | 17.5 W/m-K @Temperature 400 °C |
121 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |