Thermal Properties Metric English Comments
Thermal Conductivity 0.218 W/m-K

@Temperature 200 °C
1.51 BTU-in/hr-ft²-°F

@Temperature 392 °F
ASTM C182
BNZ Materials BNZP-26A Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..