Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.180 W/m-K @Temperature 870 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
Pyrotek M-18 Compressible/Insulating Boards ApplicationsTrough, ladle and launder linings High temperature gaskets Mill board substitute AdvantagesWater moldable Excellent thermal shock resistance High compressibility Excellent resistance to .. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 100 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1.. |
|||
Thermal Conductivity | 0.180 - 0.260 W/m-K @Temperature 600 °C |
1.25 - 1.80 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 95 Refractory Insulating Castable Description: Golite 95 is widely applied as an insulating backlining behind a dense castable, especially in the petrochemical industry.Remarks: These values apply to cast products. Also available in.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 400 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 752 °F |
BS 1902 Section 5.5 1991 |
Skamol Group Moler 10 Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 400 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 752 °F |
BS 1902 Section 5.5 1991 |
Skamol Group Moler 5 Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 400 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 752 °F |
BS 1902 Section 5.5 1991 |
Skamol Group Moler BB-Filler Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 200 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group Moler ROTOL Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 200 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group SKAMOLEX V-1100 (700) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 200 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group SKAMOLEX V-1100 (700) Panel Design SKAMOLEX panel designs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and versatil.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 200 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group SKAMOLEX V-1100 (800) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 600 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-201 supplemented by ASTM C-182 |
Skamol Group VERMICAST 116-25 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 816 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 1500 °F |
8 pcf blanket (Parallel to thickness) |
Zircar Ceramics ASB-2300 Alumina-Silica Blanket Useful to temperatures of 1260°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 200 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 392 °F |
ASTM C182 |
BNZ Materials BNZP-23B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.180 W/m-K @Thickness 0.127 mm |
1.25 BTU-in/hr-ft²-°F @Thickness 0.00500 in |
|
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.180 W/m-K @Thickness 0.127 mm |
1.25 BTU-in/hr-ft²-°F @Thickness 0.00500 in |
|
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.180 W/m-K @Thickness 0.127 mm |
1.25 BTU-in/hr-ft²-°F @Thickness 0.00500 in |
|
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.180 W/m-K @Thickness 0.127 mm |
1.25 BTU-in/hr-ft²-°F @Thickness 0.00500 in |
|
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.180 W/m-K @Thickness 0.127 mm |
1.25 BTU-in/hr-ft²-°F @Thickness 0.00500 in |
|
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.180 W/m-K @Thickness 0.127 mm |
1.25 BTU-in/hr-ft²-°F @Thickness 0.00500 in |
|
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.180 W/m-K @Thickness 0.127 mm |
1.25 BTU-in/hr-ft²-°F @Thickness 0.00500 in |
|
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.180 W/m-K @Thickness 0.127 mm |
1.25 BTU-in/hr-ft²-°F @Thickness 0.00500 in |
|
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.180 W/m-K @Thickness 0.127 mm |
1.25 BTU-in/hr-ft²-°F @Thickness 0.00500 in |
|
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.180 W/m-K @Thickness 0.127 mm |
1.25 BTU-in/hr-ft²-°F @Thickness 0.00500 in |
|
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 100 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
DuPont Performance Polymers Kalrez® 1050LF FFKM Perfluoroelastomer A general-purpose compound for O-rings, seals, and other parts used in chemical process industries. It has good hot water/steam, excellent amine resistance, and enhanced compression set properties... |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 100 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen.. |
|||
Thermal Conductivity | 0.180 W/m-K @Temperature 100 °C |
1.25 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry application.. |