Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.141 W/m-K @Temperature 400 °C |
0.979 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
3M Nextel™ BF-30 Woven Fabric 440 Information provided by 3M |