Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.870 W/m-K @Temperature 700 °C |
6.04 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Pyrotek Pyrocast AR PLUS Castable Refractory Pyrocast AR Plus is a fused silica refractory castable inert to molten aluminum and its alloys. Parts cast from Pyrocast AR Plus are heat-treated to ensure that free and combined water are removed... |
|||
Thermal Conductivity | 0.870 - 0.970 W/m-K @Temperature 1000 °C |
6.04 - 6.73 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast CURON 150 RN Dense Refractory Castable Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast .. |
|||
Thermal Conductivity | 0.870 - 0.970 W/m-K @Temperature 100 °C |
6.04 - 6.73 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 120 S Dense Refractory Castable Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in .. |
|||
Thermal Conductivity | 0.870 - 0.970 W/m-K @Temperature 600 °C |
6.04 - 6.73 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 13 S Dense Refractory Castable Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol.. |
|||
Thermal Conductivity | 0.870 - 0.970 W/m-K @Temperature 600 °C |
6.04 - 6.73 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 13 SC Dense Refractory Castable Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/ho.. |
|||
Thermal Conductivity | 0.870 - 0.970 W/m-K @Temperature 600 °C |
6.04 - 6.73 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 14 S Dense Refractory Castable Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem.. |