Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.370 W/m-K @Temperature 100 °C |
2.57 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Pyrotek NAD-11 Structural Insulation Board NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation .. |
|||
Thermal Conductivity | 0.370 W/m-K @Temperature 1095 °C |
2.57 BTU-in/hr-ft²-°F @Temperature 2003 °F |
|
Pyrotek SF-50 Foamed Fused Silica Insulation Board SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o.. |
|||
Thermal Conductivity | 0.370 W/m-K @Temperature 250 °C |
2.57 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Thermal Conductivity | 0.370 - 0.470 W/m-K @Temperature 100 °C |
2.57 - 3.26 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu.. |
|||
Thermal Conductivity | 0.370 - 0.470 W/m-K @Temperature 200 °C |
2.57 - 3.26 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Gouda Vuurvast FI 45-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.370 - 0.470 W/m-K @Temperature 100 °C |
2.57 - 3.26 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 125 GM Refractory Insulating Castable Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast... |
|||
Thermal Conductivity | 0.370 - 0.470 W/m-K @Temperature 600 °C |
2.57 - 3.26 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 135 Refractory Insulating Castable Description: Golite 135 can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning vari.. |
|||
Thermal Conductivity | 0.370 W/m-K @Temperature 1093 °C |
2.57 BTU-in/hr-ft²-°F @Temperature 1999 °F |
ASTM C182 |
BNZ Materials BNZ-26 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.370 W/m-K @Temperature 816 °C |
2.57 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials BNZ-28 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.370 W/m-K @Temperature 1000 °C |
2.57 BTU-in/hr-ft²-°F @Temperature 1830 °F |
ASTM C182 |
BNZ Materials Color A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.370 W/m-K @Temperature 1093 °C |
2.57 BTU-in/hr-ft²-°F @Temperature 1999 °F |
ASTM C182 |
BNZ Materials PA 23 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.370 - 0.470 W/m-K @Temperature 100 °C |
2.57 - 3.26 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 135 GM Refractory Insulating Castable Description: This gunning material can be used in direct contact with open fire and has a high strength.Remarks: These values were obtained from cast samples. These values apply to cast products.Inf.. |