Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.218 W/m-K @Temperature 200 °C |
1.51 BTU-in/hr-ft²-°F @Temperature 392 °F |
ASTM C182 |
BNZ Materials BNZP-26A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |