Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0260 W/m-K @Temperature 500 °C |
0.180 BTU-in/hr-ft²-°F @Temperature 932 °F |
@ 320 kg/m³; ASTM C177, ISO 8302 |
Microtherm Group Molded Pipe Sections Filament Reinforced Silica Pipe Insulation Microtherm® Moulded Pipe Sections (MPS) are preformed pieces of pipe insulation designed to provide a thermally efficient insulation system for piping of all sizes from 25 mm (1â€) upwards. F.. |
|||
Thermal Conductivity | 0.0259 W/m-K @Temperature 816 °C |
0.180 BTU-in/hr-ft²-°F @Temperature 1500 °F |
8 pcf blanket (Parallel to Thickness) |
Zircar Ceramics ASB-2600 Alumina-Silica Blanket Useful to temperatures of 1400°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics. |