Polymer Property : Thermal Conductivity = 0.120 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.120 W/m-K

@Temperature 200 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 392 °F
Pyrotek Pyrite N-14 Refractory Board
Pyrotek N-14 is a fiberglass reinforced calcium silicate board specifically developed for the non-ferrous industry. The superior strength and unique formulation of Pyrotek N-14 makes it the preferr..
Thermal Conductivity 0.120 W/m-K

@Temperature 482 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 900 °F
Pyrotek Pyrotherm TF-19 Lightweight, non-RCF insulation board for ovens, furnaces, kilns and vessels
Pyrotherm TF-19 is a high-temperature board providing high strength and excellent workability. It is composed of mineral fiber and selected mineral additives.ApplicationsPot cradle insulation (for ..
Thermal Conductivity 0.120 - 0.180 W/m-K

@Temperature 815 °C
0.833 - 1.25 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Gouda Vuurvast GOLITE 90 L Refractory Insulating Castable
Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning ..
Thermal Conductivity 0.120 W/m-K

@Temperature 400 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-182
Skamol Group ISOPERLOR 550P Perlite Insulating Brick & Block
ISOPERLOR perlite insulating bricks & blocks have the following characteristics: Max. service temperature 900°C (1652°F)Back-up insulation onlyExcellent insulating propertiesVery lightweight a..
Thermal Conductivity 0.120 W/m-K

@Temperature 400 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-182
Skamol Group Moler HIPOROS Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Thermal Conductivity 0.120 W/m-K

@Temperature 200 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
Skamol Group V-1100 375 Vermiculite Insulating Slab
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr..
Thermal Conductivity 0.120 W/m-K

@Temperature 200 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
Skamol Group V-LITE 375 Vermiculite Insulating Brick
V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica..
Thermal Conductivity 0.120 W/m-K

@Temperature 525 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 977 °F
Parallel to thickness; ASTM C177-76
Zircar Ceramics AL-30 Alumina Insulation
AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C..
Thermal Conductivity 0.120 W/m-K

@Temperature 525 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 977 °F
parallel to thickness; ASTM C177-76
Zircar Ceramics AL-30AAH Alumina Insulation
AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics.
Thermal Conductivity 0.120 W/m-K

@Temperature 800 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics ZAL-15AA Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.
Thermal Conductivity 0.120 W/m-K

@Temperature 427 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 801 °F
Zircar Refractory Composites RS-99-45 Refractory Sheet
ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani..
Thermal Conductivity 0.120 W/m-K

@Temperature 200 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 392 °F
parallel to thickness
Zircar Refractory Composites ZIRCAL-45 Refractory Board
Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength com..
Thermal Conductivity 0.120 W/m-K

@Temperature 400 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 752 °F
parallel to thickness
Zircar Refractory Composites ZIRCAL-45 Refractory Board
Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength com..
Thermal Conductivity 0.120 W/m-K

@Temperature 600 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 1110 °F
parallel to thickness
Zircar Refractory Composites ZIRCAL-45 Refractory Board
Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength com..
Thermal Conductivity 0.120 W/m-K

@Temperature 800 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Zircar Refractory Composites ASPA-880 Alumina-Silica Fiber Paper
ASPA-880 is a high temperature, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. It is made from shorter and smaller diameter fibers with a higher ..
Thermal Conductivity 0.120 W/m-K

@Temperature 800 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Zircar Refractory Composites ASPA-970 Alumina-Silica Fiber Paper
ASPA-970 is an industrial grade, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conduct..
Thermal Conductivity 0.120 W/m-K

@Temperature 204 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 399 °F
BNZ Materials Marinite® I&M High Temperature Structural Insulation
Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating..
Thermal Conductivity 0.120 W/m-K

@Temperature 427 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 801 °F
BNZ Materials Marinite® I&M High Temperature Structural Insulation
Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating..
Thermal Conductivity 0.120 W/m-K

@Temperature 538 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 1000 °F
BNZ Materials Marinite® I&M High Temperature Structural Insulation
Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating..
Thermal Conductivity 0.120 W/m-K

@Temperature 525 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 977 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics AL-30AA Alumina Insulation
AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C..
Thermal Conductivity 0.120 W/m-K

@Temperature 800 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics ZAL-15 Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.