Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0222 W/m-K @Temperature 200 °C |
0.154 BTU-in/hr-ft²-°F @Temperature 392 °F |
@ 320 kg/m³; ASTM C177, ISO 8302 |
Microtherm Group Molded Pipe Sections Filament Reinforced Silica Pipe Insulation Microtherm® Moulded Pipe Sections (MPS) are preformed pieces of pipe insulation designed to provide a thermally efficient insulation system for piping of all sizes from 25 mm (1â€) upwards. F.. |