Polymer Property : Vicat Softening Point = 99.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 99.0 °C

@Load 1.02 kg
210 °F

@Load 2.25 lb
ISO 306/A 120
Polimeri Europa Sinkral® PD L 322 ABS Resin
Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and..
Vicat Softening Point 99.0 °C

@Load 5.001 kg
210 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH 150DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Vicat Softening Point 99.0 °C

@Load 1.02 kg
210 °F

@Load 2.25 lb
50°C per hour; ISO 306A50
Total Polystyrene Impact 8260 Improved Environmental Stress Crack Resistance High Impact Polystyrene
POLYSTYRENE IMPACT 8260 is a high impact polystyrene for extrusion and injection applications. This grade has an improved environmental stress crack resistance in comparison with standard high impa..
Vicat Softening Point 99.0 °C

@Load 0.999 kg
210 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASTIR HI 0408 V0 Flame Retardant Polystyrene
Flame retardant class V0, PBDE free, good impact resistance, good thermal resistance, high light resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 99.0 °C

@Load 0.999 kg
210 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASTIR HI 0508 V0 Flame Retardant Polystyrene
Flame retardant class V0, PBDE free, good impact resistance, good thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 99.0 °C

@Load 0.999 kg
210 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASTIR HI 10 V0 Flame Retardant Polystyrene
Flame retardant class V0, with PBDE, for injection molding or extrusionInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 99.0 °C

@Load 5.00 kg
210 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-717C ABS
Medium impact
Vicat Softening Point 99.0 °C

@Load 1.00 kg
210 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-737 ABS - High Flow
High flow, medium impact
Vicat Softening Point 99.0 °C

@Load 5.00 kg
210 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PH-60 Polystyrene - High Impact
Medium impact
Vicat Softening Point 99.0 °C

@Load 1.00 kg
210 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Kibiton® PB-5900 Styrene-Butadiene Copolymer
Injection Molding, High rigidity
Vicat Softening Point 99.0 °C

@Load 1.00 kg
210 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-764 ABS - Flame Retardant
F.R. Weather Resistant
Vicat Softening Point 99.0 °C

@Load 1.00 kg
210 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-764B ABS - Flame Retardant
F.R. Weather Resistant
Vicat Softening Point 99.0 °C

@Load 1.00 kg
210 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-764B ABS - Flame Retardant
F.R. Weather Resistant
Vicat Softening Point 99.0 °C

@Load 5.00 kg
210 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Wonderloy® PC-540 PC/ABS Alloy - Flame Retardant
High Heat