Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 85.0 °C @Load 5.001 kg |
185 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs V0X ABS, Flame Retardant Information provided by Polykemi AB |
|||
Vicat Softening Point | 85.0 °C @Load 5.001 kg |
185 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH BK901213 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 85.0 °C @Load 5.00 kg |
185 °F @Load 11.0 lb |
50°C/min; ASTM D1525 |
Kingfa HF-618 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Vicat Softening Point | 85.0 °C @Load 5.10 kg |
185 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 3150 Polypropylene, Homopolymer Polypropylene PPH 3150 is a modified homopolymer polypropylene with a Melt Flow index of 2 g/10 min.Polypropylene PPH 3150 is intended for the production at very high speed of flat bioriented films .. |
|||
Vicat Softening Point | 85.0 °C @Load 5.10 kg |
185 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 4030 Polypropylene Homopolymer Polypropylene PPH 4030 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4030 has been designed for the production of BOPP film with the tenter frame process. Th.. |
|||
Vicat Softening Point | 85.0 °C @Load 5.10 kg |
185 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 4054 Polypropylene Homopolymer Polypropylene PPH 4054 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4054 has been designed for the production of BOPP film with the tenter frame process. Th.. |
|||
Vicat Softening Point | 85.0 °C @Load 5.10 kg |
185 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 4069 Polypropylene Homopolymer, Fiber Polypropylene PPH 4069 is a homopolymer polypropylene with a Melt Flow index of 4 g/10 min.Polypropylene PPH 4069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Vicat Softening Point | 85.0 °C @Load 5.10 kg |
185 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 5069 Polypropylene Homopolymer, Fiber Polypropylene PPH 5069 is a homopolymer polypropylene with a Melt Flow index of 6 g/10 min.Polypropylene PPH 5069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Vicat Softening Point | 85.0 °C @Load 5.00 kg |
185 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 1218 V0/B Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 85.0 °C @Load 5.00 kg |
185 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-764B ABS - Flame Retardant F.R. Weather Resistant |