Polymer Property : Vicat Softening Point = 79.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 79.0 °C

@Load 5.00 kg
174 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-765A ABS - Flame Retardant
F.R. High Flow
Vicat Softening Point 79.0 °C

@Load 5.00 kg
174 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-765B ABS - Flame Retardant
F.R. Medium Impact
Vicat Softening Point 79.0 °C

@Load 5.001 kg
174 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC GF5020 Polypropylene Copolymer, Glass Fiber Reinforced
Information provided by Polykemi AB