Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 76.0 °C @Load 5.001 kg |
169 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC TS4030 H Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 76.0 °C @Load 5.001 kg |
169 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC K3020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 76.0 °C @Load 5.10 kg |
169 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 165 N/L GPPS Styrolution PS 165N/L is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.High molecular weightGood flow characteristicsAppropriate for blending with HIPS.. |
|||
Vicat Softening Point | 76.0 °C @Load 5.10 kg |
169 °F @Load 11.2 lb |
50°C per hour; ISO 306B50 |
Total PS CPDS 9217 Compound Polystyrene/Polyethylene POLYSTYRENE (PS) COMPOUND (CPDS) 9217 is an alloy of polystyrene and polyethylene. This combination brings the benefits of polyethylene; a high level of stress crack resistance, mechanical properti.. |
|||
Vicat Softening Point | 76.0 °C @Load 5.00 kg |
169 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Kibiton® PB-5900 Styrene-Butadiene Copolymer Injection Molding, High rigidity |
|||
Vicat Softening Point | 76.0 °C @Load 5.001 kg |
169 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC K5020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 76.0 °C @Load 5.001 kg |
169 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC K8020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 76.0 °C @Load 5.001 kg |
169 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC K9020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |