Polymer Property : Vicat Softening Point = 73.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 73.0 °C

@Load 5.001 kg
163 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PP EIP5025 F VT2 Polypropylene, Mineral Reinforced, Extrusion grade, Low CLTE
Information provided by Polykemi AB
Vicat Softening Point 73.0 °C

@Load 5.001 kg
163 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC T20040 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 73.0 °C

@Load 5.00 kg
163 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Kibiton® PB-5925 SBC
Transparency, high stiffness, injection grade