Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 200 °C @Load 5.001 kg |
392 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYshine PBT D221 QF30 PBT, Glass and Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 200 °C @Load 5.001 kg |
392 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANMID 6 B12^ NH6 Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Vicat Softening Point | 200 °C @Load 5.001 kg |
392 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANMID 6 B12^ NH9 Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Vicat Softening Point | 200 °C @Load 5.001 kg |
392 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANMID 6 B12^ NH9L Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Vicat Softening Point | 200 °C @Load 5.001 kg |
392 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANMID 6 B12^ Nylon 6 Information provided by Polykemi AB |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Lanxess Durethan® B 40 SK 000000 Nylon 6 PA 6, non-reinforced, injection molding |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Lanxess Durethan® B 40 SK 000000 Nylon 6 PA 6, non-reinforced, injection molding |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
120°C/hour; ISO 306 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
50°C/hour; ISO 306 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
Vicat Softening Point | >= 200 °C @Load 5.10 kg |
>= 392 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Vicat Softening Point | >= 200 °C @Load 5.10 kg |
>= 392 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Vicat Softening Point | >= 200 °C @Load 5.10 kg |
>= 392 °F @Load 11.2 lb |
120°C/hour; ISO 306 |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
Vicat Softening Point | >= 200 °C @Load 5.10 kg |
>= 392 °F @Load 11.2 lb |
50°C/hour; ISO 306 |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
cond.; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T.. |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
dry; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
cond.; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
cond.; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
cond.; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
dry; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 MCS V0 Polyamide 6 - Flame Retarded, Unreinforced Flame retarded (class V0), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th.. |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
dry; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 MCS V2 Polyamide 6 - Flame Retarded, Unreinforced Flame retarded (class V2), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th.. |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
dry; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 MX6 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% hybrid mineral-glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good su.. |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
cond.; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 GF40 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 40% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Vicat Softening Point | 200 °C @Load 5.10 kg |
392 °F @Load 11.2 lb |
cond.; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |