Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 136 °C @Load 1.00 kg |
277 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB SCANBLEND FS7 PC/ASA Blend with Improved Weather Resistance Information provided by Polykemi AB |
|||
Vicat Softening Point | 136 °C @Load 1.00 kg |
277 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB SCANBLEND FS7 UV4 PC/ASA Blend with Improved Weather Resistance Information provided by Polykemi AB |
|||
Vicat Softening Point | 136 °C @Load 1.02 kg |
277 °F @Load 2.25 lb |
ISO 306 |
Borealis Daplen™ EE188AI Polypropylene TPO Compound Daplen™ EE188AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Vicat Softening Point | 136 °C @Load 1.02 kg |
277 °F @Load 2.25 lb |
ISO 306 |
Borealis Daplen™ EE189AI Polypropylene TPO Compound Daplen™ EE189AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Vicat Softening Point | 136 °C @Load 5.10 kg |
277 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® FR3050 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Vicat Softening Point | 136 °C @Load 1.00 kg |
277 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Wonderloy® PC-365 PC/ABS Alloy High Heat, High Impact |
|||
Vicat Softening Point | 136 °C @Load 1.00 kg |
277 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC EP1001F Polypropylene Information provided by Polykemi AB |