Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 121 °C @Load 1.02 kg |
250 °F @Load 2.25 lb |
ISO 306 |
Borealis Daplen™ EF005AE Polypropylene TPO Compound Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Vicat Softening Point | 121 °C @Load 5.00 kg |
250 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 0815 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood melt flow rate, good impact resistance, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 121 °C @Load 0.999 kg |
250 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 1030 HT V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good light resistance, good processability and surface appearanceInformation provided by Cossa Polimeri S.. |
|||
Vicat Softening Point | 121 °C @Load 5.10 kg |
250 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® T65 AT PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
Vicat Softening Point | 121 °C @Load 5.00 kg |
250 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-777E ABS - High Heat Ultra High Heat |