Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 230 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 110 °C

@Load 5.001 kg
230 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYblend 6005 PC/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 110 °C

@Load 5.001 kg
230 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYblend 6005B PC/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 110 °C

@Load 5.001 kg
230 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYblend 6005B UV PC/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 110 °C

@Load 1.00 kg
230 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYelast TPE ZC100 D40 Thermoplastic Elastomer
Information provided by Polykemi AB
Vicat Softening Point 110 °C

@Load 5.001 kg
230 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYplex PMMA 500 Acrylic Glass
Information provided by Polykemi AB
Vicat Softening Point 110 °C

@Load 5.001 kg
230 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYlux 3809S FR PC/PBT-Blend, Flame Retardant
Information provided by Polykemi AB
Vicat Softening Point 110 °C

@Load 5.00 kg
230 °F

@Load 11.0 lb
50°C/min; ASTM D1525
Kingfa HR-527B Modified ABS
Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd...
Vicat Softening Point 110 °C

@Load 5.00 kg
230 °F

@Load 11.0 lb
50°C/hour; ISO 306
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade
Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®..
Vicat Softening Point 110 °C

@Load 5.10 kg
230 °F

@Load 11.2 lb
50°C/h; ISO 306
Styrolution Terblend® S NM-31 ASA / PA
Terblend® S is a UV-stabilized ASA/PA blend with high impact strength, easy flow and pronounced color fastness. It is especially suitable for unpainted highly UV-exposed automotive interior parts..
Vicat Softening Point 110 °C

@Load 5.00 kg
230 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTABLEND 7500 V0 HF Flame Retardant PC - ABS
PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, good thermal and mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l..
Vicat Softening Point 110 °C

@Load 5.00 kg
230 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTABLEND CR Polycarbonate ABS Blend
Polycarbonate and Acrylonitrile Butadiene Styrene blend for chromium plating, painting and metallizationGood impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 110 °C

@Load 5.00 kg
230 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1030 HT V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good light resistance, good processability and surface appearanceInformation provided by Cossa Polimeri S..
Vicat Softening Point 110 °C

@Load 0.999 kg
230 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 2020 MT Acrylonitrile Butadiene Styrene
ABSMedium heat resistance, good impact resistance, good melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 110 °C

@Load 0.999 kg
230 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 3008 MT Acrylonitrile Butadiene Styrene
ABS with very high impact resistanceHigh impact resistance at low temperature, medium heat resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 110 °C

@Load 0.999 kg
230 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 3015 MT Acrylonitrile Butadiene Styrene
ABSMedium thermal resistance, high impact resistance at low temperature, good melt flow rate, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 110 °C

@Load 5.10 kg
230 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® FR3100 TV PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 110 °C

@Load 5.10 kg
230 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® FR3110 TV PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 110 °C

@Load 5.10 kg
230 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® R-FR610 Polycarbonate Recyclate Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame retardantAs of 1 S..
Vicat Softening Point 110 °C

@Load 1.00 kg
230 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-127 SAN
Heat Resistant
Vicat Softening Point 110 °C

@Load 1.00 kg
230 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PG-383 Polystyrene
High heat; high strength
Vicat Softening Point 110 °C

@Load 0.999 kg
230 °F

@Load 2.20 lb
120°C/min; ASTM D1525/A, ISO 306/A
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber
Characteristics: 17% glass fibre filled
Vicat Softening Point 110 °C

@Load 1.00 kg
230 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-127H SAN
Chemical Resistant
Vicat Softening Point 110 °C

@Load 5.00 kg
230 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Wonderloy® PC-345 PC/ABS Alloy
High Flow
Vicat Softening Point 110 °C

@Load 1.00 kg
230 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYabs F00 GF17 ABS, Glass Fiber-Reinforced
Information provided by Polykemi AB
Vicat Softening Point 110 °C

@Load 5.001 kg
230 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs H00 ABS, Heat Resistant
Information provided by Polykemi AB
Copyright © lookpolymers.com All Rights Reserved