Polymer Property : Vicat Softening Point = 196 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 91.0 °C

@Thickness 4.00 mm
196 °F

@Thickness 0.157 in
Rate A; ISO 306/B50
Premix Thermoplastics PRE-ELEC® ABS 1410
PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141..
Vicat Softening Point 91.0 °C

@Load 5.00 kg
196 °F

@Load 11.0 lb
50°C/min; ASTM D1525
Kingfa FW-650 Flame Retardant ABS
Features:Weather resistanceSuper high impact resistanceApplications:Injection moldingSwitchSocketInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 91.0 °C

@Load 1.02 kg
196 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution PS 454N HIPS
Styrolution PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Good balance of toughness, high flow, and heat resistanceHigh gloss..
Vicat Softening Point 91.0 °C

@Load 5.00 kg
196 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASTIR HI 0408 V0 Flame Retardant Polystyrene
Flame retardant class V0, PBDE free, good impact resistance, good thermal resistance, high light resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 91.0 °C

@Load 5.10 kg
196 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Bayblend® FR3210 TV PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 91.0 °C

@Load 1.00 kg
196 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-765A ABS - Flame Retardant
F.R. High Flow
Vicat Softening Point 91.0 °C

@Load 5.00 kg
196 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PG-22 Polystyrene
TPE compound
Vicat Softening Point 91.0 °C

@Load 5.00 kg
196 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PH-888G Polystyrene - High gloss
High impact; high gloss
Vicat Softening Point 91.0 °C

@Load 5.00 kg
196 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-746H ABS - High Flow
Super high flow, medium impact