Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 90.0 °C @Load 5.001 kg |
194 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CIM9040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 90.0 °C @Load 5.001 kg |
194 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GK8040 Polypropylene Homopolymer, Glass Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 90.0 °C @Load 5.001 kg |
194 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC GF3020 PB7 Polypropylene, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 90.0 °C @Load 5.001 kg |
194 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T4060 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 90.0 °C @Load 1.00 kg |
194 °F @Load 2.20 lb |
120°C/min; ASTM D1525 |
Kingfa NH-627 Flame Retardant ABS Features:UL 94 V-2 @ 1.6mmHalogen-free flame retardantHigh flowApplications:OA deviceDigital cameraVidiconInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution PS 476L HIPS Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl.. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 486N HIPS Styrolution PS 486N is a normal flowing, high impact grade that is especially suitable for blends with a high proportion of general purpose polystyrene (preferably Styrolution PS 165N of Styrolution.. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution PS 495F HIPS Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection.. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution PS 576H HIPS Styrolution PS 576H is a high gloss, high impact polystyrene with a good flow and good heat resistance.High gloss HIPSGood flow and heat resistanceHIPS with good balance of mechanical properties and.. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
ISO 306 |
Borealis HB601WG Polypropylene Homopolymer HB601WG is a polypropylene homopolymer intended for injection molding and blow molding. The product is available in natural but other colors can be provided on request. This material has excellent .. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
ISO 306 |
Borealis HF700SA Polypropylene HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor.. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
50°C per hour; ISO 306B50 |
Total Polystyrene Impact 8260 Improved Environmental Stress Crack Resistance High Impact Polystyrene POLYSTYRENE IMPACT 8260 is a high impact polystyrene for extrusion and injection applications. This grade has an improved environmental stress crack resistance in comparison with standard high impa.. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 12020 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 12020 is a clarified high fluidity homopolymer with a melt flow index of 60 g/10 min.Polypropylene PPH 12020 has been designed with a very high stiffness and an outstanding transpa.. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 4070 Polypropylene Homopolymer Polypropylene PPH 4070 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4070 has been designed for the production of BOPP film with the tenter frame process and .. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTALUX 9206 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTALUX 9206 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information.. |
|||
Vicat Softening Point | 90.0 °C @Load 1.00 kg |
194 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-765A ABS - Flame Retardant F.R. High Flow |
|||
Vicat Softening Point | 90.0 °C @Load 1.00 kg |
194 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-765 ABS - Flame Retardant F.R. High Flow |
|||
Vicat Softening Point | 90.0 °C @Load 1.00 kg |
194 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-765 ABS - Flame Retardant F.R. High Flow |
|||
Vicat Softening Point | 90.0 °C @Load 1.00 kg |
194 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-765B ABS - Flame Retardant F.R. Medium Impact |
|||
Vicat Softening Point | 90.0 °C @Load 5.001 kg |
194 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T5060 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |