Polymer Property : Vicat Softening Point = 154 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 68.0 °C

@Load 5.001 kg
154 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PP CQX15015 R3 UV Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
Vicat Softening Point 68.0 °C

@Load 5.001 kg
154 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANFILL BOTTLE BY45C2 Blow Molding Grade
Information provided by Polykemi AB
Vicat Softening Point 68.0 °C

@Load 5.00 kg
154 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Kibiton® PB-5903 SBC
High transparency, high toughness, PS Impact modifier
Vicat Softening Point 68.0 °C

@Load 5.001 kg
154 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC 15000 Polypropylene Copolymer
Information provided by Polykemi AB