Polymer Property : Vicat Softening Point = 123 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C

@Load 5.001 kg
253 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANBLEND FS7 PC/ASA Blend with Improved Weather Resistance
Information provided by Polykemi AB
Vicat Softening Point 123 °C

@Load 5.001 kg
253 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANBLEND FS7 UV4 PC/ASA Blend with Improved Weather Resistance
Information provided by Polykemi AB
Vicat Softening Point 123 °C

@Load 0.999 kg
253 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTABLEND CR Polycarbonate ABS Blend
Polycarbonate and Acrylonitrile Butadiene Styrene blend for chromium plating, painting and metallizationGood impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 123 °C

@Load 5.00 kg
253 °F

@Load 11.0 lb
120°C/hr; ASTM D 1525
Cossa Polimeri ESTABLEND PSA 6600 PC / ASA Blend
Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 123 °C

@Load 0.999 kg
253 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1016 HT V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim..
Vicat Softening Point 123 °C

@Load 0.999 kg
253 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1218 HT V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearance, high thermal resistanceInformation provided by Cossa Po..
Vicat Softening Point 123 °C

@Load 5.00 kg
253 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Wonderloy® PC-365 PC/ABS Alloy
High Heat, High Impact
Vicat Softening Point 123 °C

@Load 1.02 kg
253 °F

@Load 2.25 lb
ISO 306
Addcomp PRIEX® 12031 Maleic Anhydride Grafted HDPE
Fields of application: Functionalised polyethylene to be used as compatibiliser for polymer blends or coupling agent for wood flour, natural fibres, or mineral filled polyolefins. Also suitable to r..