Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 121 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 121 °C

@Load 1.02 kg
250 °F

@Load 2.25 lb
ISO 306
Borealis Daplen™ EF005AE Polypropylene TPO Compound
Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give..
Vicat Softening Point 121 °C

@Load 5.00 kg
250 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 0815 HHT Acrylonitrile Butadiene Styrene
ABS with very high heat resistanceGood melt flow rate, good impact resistance, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 121 °C

@Load 0.999 kg
250 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1030 HT V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good light resistance, good processability and surface appearanceInformation provided by Cossa Polimeri S..
Vicat Softening Point 121 °C

@Load 5.10 kg
250 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® T65 AT PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp..
Vicat Softening Point 121 °C

@Load 5.00 kg
250 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-777E ABS - High Heat
Ultra High Heat