Thermal Properties Metric English Comments
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYasa 1614F UV-resistant ASA
Information provided by Polykemi AB
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYasa 2008F UV-stabilized, High Flow ASA
Information provided by Polykemi AB
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYasa 2410F High Flow ASA
Information provided by Polykemi AB
Vicat Softening Point 103 °C

@Load 5.001 kg
217 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYblend 45FS GKF2505 PC/ABS-Blend, Glass Fiber reinforced
Information provided by Polykemi AB
Vicat Softening Point 103 °C

@Load 5.001 kg
217 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs F00 GF15 ABS, Glass Fiber-Reinforced
Information provided by Polykemi AB
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.20 lb
120°C/min; ASTM D1525
Kingfa FW-620 Flame Retardant ABS
Features:UL 94 V-0 @ 1.5-3.0mmWeather resistanceHeat resistanceGood surfaceApplications:Injection moldingOA deviceChargerTransformerInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.20 lb
120°C/min; ASTM D1525
Kingfa HC-110 Modified ABS
Features:UL94 HB @ 1.6-3.0mmElectro-platingApplications:Electro-plating partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 103 °C

@Load 5.00 kg
217 °F

@Load 11.0 lb
50°C/min; ASTM D1525
Kingfa HR-527A Modified ABS
Features:UL94 HB @ 1.5-3.2mmHeat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 103 °C

@Load 1.02 kg
217 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution Terluran® GP-25 ABS
Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se..
Vicat Softening Point 103 °C

@Load 1.02 kg
217 °F

@Load 2.25 lb
50°C per hour; ISO 306A50
Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene
POLYSTYRENE IMPACT 3450 is a high impact polystyrene with high heat resistance, good flow, high stiffness and good aesthetics. With such an ideal balance of properties, POLYSTYRENE IMPACT 3450 is w..
Vicat Softening Point 103 °C

@Load 0.999 kg
217 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1030 V0/F Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high melt flow rate, good impact resistance, high gloss, good light resistance, excellent processabilityInformation provided by Co..
Vicat Softening Point 103 °C

@Load 0.999 kg
217 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1050 AS Acrylonitrile Butadiene Styrene
General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 103 °C

@Load 5.10 kg
217 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® FR3009 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 103 °C

@Load 5.00 kg
217 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-106 L150 SAN
High Clarity
Vicat Softening Point 103 °C

@Load 5.00 kg
217 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-107 L125 SAN
High Clarity
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-709 ABS
Super impact
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-716 ABS - High Flow
High flow, medium impact
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-717C ABS
Medium impact
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-726 ABS
Electro-plating
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-726 ABS
Electro-plating
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-746 ABS - High Flow
High flow, medium impact
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-747 ABS
High impact
Vicat Softening Point 103 °C

@Load 5.00 kg
217 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PG-383 Polystyrene
High heat; high strength
Vicat Softening Point 103 °C

@Load 5.00 kg
217 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASAN SAN 0840 GF Styrene Acrylonitrile
SAN with 20% glass fiber reinforcementExcellent dimensional stability, good heat resistanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-747S ABS - Extrusion
High Impact Extrusion
Vicat Softening Point 103 °C

@Load 1.00 kg
217 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-763 ABS - Flame Retardant
F.R. High Heat Weather Resistant