Polymer Property : Vicat Softening Point = 100 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs S00 ABS, High Flow
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs S00 AS UV ABS, High Flow, UV-Stabilized, Antistatic
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs S00 GK10 ABS, High Flow
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs SN0 ABS
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs SS0 ABS, High Flow
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs X00 ABS, Extrusion Grade
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs XX0 ABS, Extrusion Grade
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYblend 45FS GK25 PC/ABS-Blend, Glass Fiber reinforced
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYsan PN127 Styrene Acrylonitrile
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs F00 ABS
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs F20 ABS
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs F30 ABS
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH B8065 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH B8065 VT1 Polypropylene Homopolymer, Mineral Reinforced, Heat Resistant
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 5.001 kg
212 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYplex PMMA 700 Acrylic Glass
Information provided by Polykemi AB
Vicat Softening Point 100 °C

@Load 1.02 kg
212 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution Novodur® BX13036 ABS + PMMA
Novodur BX13036 is a new PMMA/ABS blend with high surface quality, enhanced scratch resistance and balanced mechanical propertiesInformation provided by Styrolution
Vicat Softening Point 100 °C

@Load 1.02 kg
212 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution PS 147F GPPS
Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro..
Vicat Softening Point 100 °C

@Load 5.10 kg
212 °F

@Load 11.2 lb
ISO 306
Borealis MD441U Polypropylene Compound, Mineral Filled
MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond..
Vicat Softening Point 100 °C

@Load 5.10 kg
212 °F

@Load 11.2 lb
ISO 306
Borealis ME212U Polypropylene Compound, Mineral Filled
ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air..
Vicat Softening Point 100 °C

@Load 5.00 kg
212 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 3008 MT Acrylonitrile Butadiene Styrene
ABS with very high impact resistanceHigh impact resistance at low temperature, medium heat resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 100 °C

@Load 5.10 kg
212 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Bayblend® FR3012 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 100 °C

@Load 1.00 kg
212 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PH-55Y Polystyrene - Food
Medium impact
Vicat Softening Point 100 °C

@Load 1.00 kg
212 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PH-60 Polystyrene - High Impact
Medium impact
Vicat Softening Point 100 °C

@Load 1.00 kg
212 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PH-888G Polystyrene - High gloss
High impact; high gloss
Vicat Softening Point 100 °C

@Load 1.00 kg
212 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PH-88S Polystyrene - Extrusion
Extrusion
Vicat Softening Point 100 - 155 °C

@Load 0.999 kg
212 - 311 °F

@Load 2.20 lb
120°C/min; ASTM D1525/A, ISO 306/A
EPICHEM Epicarb PC BLACK IQ Polycarbonate
Characteristics: good fluidity, good impact, industrial quality
Vicat Softening Point 100 °C

@Load 5.00 kg
212 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber
Characteristics: 17% glass fibre filled
Vicat Softening Point 100 °C

@Load 5.00 kg
212 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-707 ABS
High gloss, high rigid
Vicat Softening Point 100 °C

@Load 5.00 kg
212 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-757 ABS
High gloss, medium impact
Vicat Softening Point 100 °C

@Load 1.00 kg
212 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PG-80N Polystyrene
High strength