Polymer Property : Maximum Service Temperature, Air = 79.4 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 79.4 °C
175 °F
Continuous
NOVA Chemicals Dylite® F271TN Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..
Maximum Service Temperature, Air 79.4 °C
175 °F
Continuous
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..
Maximum Service Temperature, Air 79.4 °C
175 °F
Alcoa KAMA 2100 Prime Clear OPS, Film  (discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
Maximum Service Temperature, Air 79.4 °C
175 °F
Alcoa KAMA 2200 Prime Graphic Arts OPS  (discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
Maximum Service Temperature, Air 79.4 °C
175 °F
Alcoa KAMA 2500 Prime Clear OPS, Shrink Film  (discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
Maximum Service Temperature, Air 79.4 °C
175 °F
Alcoa KAMA 2700 OPS Lamination, Film  (discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
Maximum Service Temperature, Air 79.4 °C
175 °F
dry
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear
Information provided by ITW Devcon
Maximum Service Temperature, Air 79.4 °C
175 °F
Saint-Gobain Tygothane® C-210-A Precision Polyurethane Tubing Formulation
Description: Tygothane® C-210-A: Our rigidly controlled manufacturing process makes Tygothane® Precision Polyurethane Tubing the flexible polyurethane tubing that has consistently tight toleranc..