Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 79.0 °C | 174 °F | Deflection temperature; load unknown. |
Abatron AboCast 8-15/Abocure 8-15 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/11.80 ratio (pbw); Gel time, 100 g (3.5 oz.): 70 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | See Note 2. |
ChevronTexaco Texclad® 2 Texaco Texclad 2 delivers value through:Water tolerance — Resists washout, even when subject to gross water contamination.Excellent adhesiveness — Assures good film strength even in a wet environm.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
Chesterton 740 Heavy Duty Rust Guard Description: Chesterton® 740 Heavy Duty Rust Guard is a premium quality corrosion preventative coating designed with user ease of application in mind. It is the perfect coating for those areas of t.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
3M 3320 HVAC Construction Aluminum foil/scrim/laminate. UL 723 Classified.Information provided by 3M |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
3M 3334 Aluminum Foil/Scrim/PE Facing Tape 3M™ Aluminum Foil Tape 3334 has a high performance aluminum foil/bidirectional fiberglass scrim/polyethylene film laminate backing coated with a special pressure sensitive acrylic adhesive which ex.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
3M 33803 General Purpose Aluminum Foil Tape High tack rubber adhesive. 40 lb liner. UL 723 ClassifiedInformation provided by 3M |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | Service |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | Service |
3M 7735FL Acrylate Overlaminating Film 3M™ Acrylate Overlaminating Film 7735FL utilizes an outdoor durable acrylate film facestock with exceptional UV resistance, combined with 3M™ Adhesive 400 and a film liner. This product offers exc.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
3M Safety-Walk™ 310 Black Slip-Resistant Medium Resilient Tapes and Treads A soft-textured, non-mineral, medium resilient surface bonded to a pressure-sensitive adhesive backed plastic film. For barefoot- or shoe-traffic areasNon-mineral, medium textured, slip-resistant vi.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
3M Safety-Walk™ 370 Gray Slip-Resistant Medium Resilient Tapes and Treads A soft-textured, non-mineral, medium resilient surface bonded to a pressure-sensitive adhesive backed plastic film. For barefoot- or shoe-traffic areasNon-mineral, medium textured, slip-resistant vi.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
3M Safety-Walk™ 510 Black Slip-Resistant Conformable Tapes and Treads A high-friction, slip-resistant material that has a special pressure-sensitive adhesive backed aluminum film that conforms around corners and adheres to irregular surfaces.For irregular or contoured.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
3M Safety-Walk™ 530 Safety Yellow Slip-Resistant Conformable Tapes and Treads A high-friction, slip-resistant material that has a special pressure-sensitive adhesive backed aluminum film that conforms around corners and adheres to irregular surfaces.For irregular or contoured.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
3M Safety-Walk™ 610 Black Slip-Resistant General Purpose Tapes and Treads A mineral-coated, slip-resistant material adhered by a durable resin to a pressure-sensitive adhesive backed plastic film.For light to heavy shoe-traffic areasMineral-coated, high friction slip-resi.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
3M Safety-Walk™ 710 Black Coarse Tapes and Treads Extra-large mineral particles and durable construction provide additional slip resistance in extreme conditions.For extreme, heavy traffic areasExtra-large abrasive mineral particles help provide a .. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | Deflection Temp at unknown load |
Abatron AboCast 8103-14 One-Component Epoxy AboCast 8103-14 is the lowest-viscosity one-component epoxy system with heavy-duty structural and dielectric properties. It is clear and has maximum wetting and penetration. Suggested Uses: Casting.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | Service |
3M 7604FP Primalyn™ White Vinyl Label Material 3M™ Primalyn™ White Vinyl Label Material 7604FP is a flexible vinyl providing excellent squeeze bottle performance with consistent printability. This material utilizes 3M™ Adhesive 300, which has.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | Short Term, 24 hrs |
3M 7620/7890 White Vinyl Label Material 3M™ White Vinyl Label Material 7620 / 7890 is a rigid, gloss vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick ta.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
3M 7885 Computer Imprintable Destructible Vinyl Label Material 3M™ Label Material 7885 matte white computer imprintable destructible vinyl product with 3M™ Adhesive 200 meets the requirements of permanent marking applications on metals, high surface energy pl.. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | |
3M Safety-Walk™ 770 Gray Coarse Tapes and Treads Extra-large mineral particles and durable construction provide additional slip resistance in extreme conditions.For extreme, heavy traffic areasExtra-large abrasive mineral particles help provide a .. |
|||
Maximum Service Temperature, Air | 79.0 °C | 174 °F | Service |
3M 7776 Polypropylene Label Material 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh.. |